dc.description.abstractPurpose: To compare shear bond strengths of three different self-etching adhesive systems of different pH values to enamel bleached with carbamide peroxide, treated with casein phosphopeptide-amorphous calcium phosphate (CPP-ACP), or treated with CPP-ACP subsequent to bleaching with carbamide peroxide. Materials and Methods: Thirty-six human third molars were cut into 4 sections and randomly assigned to 4 groups (n = 36): group I: no treatment; group II: bleaching; group III: CPP-ACP; group IV: bleaching and CPP-ACP. After surface treatments, the samples of each group were further divided into three subgroups (n = 12) based on the adhesive used. The adhesives Clearfil SE Bond (CSE), AdhesE (ADE), and Adper SE Plus (ADP) were applied, and resin composite cylinders with a diameter of 2 mm and a height of 4 mm were bonded to the enamel. Then the specimens were subjected to shear bond strength testing. Two-way ANOVA and a post-hoc Tukey's test were used for statistical analysis (alpha = 0.05). Results: There were significant differences between the adhesive systems (p < 0.001) and surface treatments (p < 0.001), but no significant interactions were observed between these variables (p = 0.78). The CSE adhesive system showed the highest bond strength, and the bleaching procedure reduced bond strengths (p = 0.001). Furthermore, there were no significant differences in shear bond strength values between the control and CPP groups. However, the differences between other groups were statistically significant (p < 0.05). Conclusion: Bleaching reduced shear bond strength to enamel, but CPP-ACP application did not affect the bond strength to intact and previously bleached enamel. The bond strength of adhesives with different pH values to enamel was material dependant.
dc.language.isoEnglish
dc.relation.ispartofJOURNAL OF ADHESIVE DENTISTRY
dc.subjectpH
dc.subjectself-etching adhesives
dc.subjectbleaching
dc.subjectcasein phosphopeptide-amorphous calcium phosphate
dc.subjectbond strength
dc.titleShear Bond Strength of Self-etching Adhesive Systems with Different pH Values to Bleached and/or CPP-ACP-treated Enamel
dc.typeArticle
dc.citation.volume14
dc.citation.issue5
dc.citation.spage447
dc.citation.epage452
dc.citation.indexWeb of science
dc.identifier.DOIhttps://doi.org/10.3290/j.jad.a23316